Search published articles


Showing 2 results for Fb-Tig

N. Rahimi, T. Saed,
Volume 5, Issue 2 (1-2020)
Abstract

In this study the effect of activating fluxes on the penetration depth, microstructure and microhardness of AISI316L austenitic stainless steel were evaluated by three TIG process variations (TIG, A-TIG and FB-TIG) and the results were compared together.. After selecting the optimal flux in the second stage, the effect of that on the penetration depth, microstructure and weld microhardness of  welded 316L austenitic stainless steel by A–TIG and FB-TIG methods, were evaluated and  the results were compared by the sample which was welded by TIG process. At this stage, it was found that the depth and width to depth ratio in FB-TIG method is slightly greater than the other two methods. Also in FB-TIG method, eqiaxed dendritic zone in the center line of weld is slightly greater than in A-TIG method. Study of microhardness of weld in three methods shows that in A-TIG and FB-TIG methods hardness of center line is more than TIG method.


R. Karimpoor, A. Farzadi, A. Ebrahimi ,
Volume 7, Issue 1 (8-2021)
Abstract

In the present study, effect of current, welding speed and preheat temperature during FB-TIG welding of AA5083 aluminum alloy was studied. Using the Taguchi method, 9 different tests were designed to investigate the effect of welding parameters on the penetration depth. Consistent with predictions, increasing the current and preheat temperature, and reducing the welding speed led to an increase in penetration depth. The maximum penetration depth of 8.02 mm was achieved at the current of 220 A, welding speed of 120 mm/min, and the preheat temperature of 100 °C. Taguchi analysis showed that increasing the welding current and preheat temperature had a more significant effect than the welding speed. Microstructural analysis indicated that the weld metal is fine-grained, along with coarse-grain in the HAZ of all samples. Many pores were observed in the samples with high welding speed and high welding current in the fusion zone. The sample with the highest heat input had the highest penetration depth. This sample had the highest elongation, equal to 69% of the base metal. Moreover, microhardness test demonstrated that the hardness of this sample dropped sharply from 70 Vickers to 58 Vickers in the HAZ.


Page 1 from 1     

© 2024 CC BY-NC 4.0 | Journal of Welding Science and Technology of Iran

Designed & Developed by : Yektaweb