Fasahat Mahmoud, Ali Khorram, Masoud Barekat,
Volume 9, Issue 2 (Journal OF Welding Science and Technology 2026)
Abstract
In this study, the effect of direct laser deposition parameters, including power, duty cycle, and scanning speed, on the microstructure and microhardness of Stellite 21/WC-10Co-4Cr composite coatings produced on Inconel 713LC was investigated. The results indicate that all coatings consisted of two primary phases: a low-hardness austenitic solid solution (γ-Co) and a high-hardness Cr₇C₃ carbide; the processing conditions strongly influenced their volume fraction and morphology. Reducing the scanning speed from 8.6 to 4.4 mm/s increased interaction time and heat input, accelerating carbide dissolution kinetics and forming fine, dispersed Cr₇C₃ carbides within the γ-Co matrix; this ultimately increased coating hardness by about 31% (from 551 to 723 HV). Increasing the duty cycle from 76% to 94% raised the fraction of the soft austenitic solid solution (γ-Co) due to the extended dwell time, reducing hardness by about 16% (from 754 to 630 HV). Similarly, increasing the power from 280 to 370 W—despite promoting greater homogenization—increased the fraction of austenitic solid solution due to excessive melt pool temperatures and enrichment of the melt with alloying elements, leading to a hardness decrease of approximately 12.5% (from 630 to 551 HV). At low power (280 W), solidification proceeds via a hypereutectic path characterized by coarse primary carbide phases (WC and M₆C) and severe elemental segregation, resulting in a heterogeneous microstructure. Increasing the power to 370 W alters the effective Co/(W+C) ratio in the melt, shifting the solidification path toward a fine eutectic structure (M₂₃C₆/M₇C₃ + γ-Co) with reduced interlamellar spacing and more uniform elemental distribution, enhancing microstructural homogeneity despite a slight increase in the dilution rate. Ultimately, the sample processed at 325 W with an 85% duty cycle and a speed of 6.5 mm/s was selected; it exhibited a hardness of 643 HV (a 66% increase over the substrate) and offered an optimal balance of hardness and toughness, alongside uniform carbide distribution and an absence of cracks or porosity.